Why a fast battery model collapses at 5 A: it is the salt diffusion
Doubling electrolyte diffusivity removes the SPMe battery model's 5 A collapse, within 2% of DFN; changing its conductivity treatment does not.
-
A battery model that lets salt go negative
Two battery cell designs the fast SPMe model scores near zero show negative electrolyte concentration, while the full DFN model stays positive.
-
Why a fast battery model gave up on thick electrodes: its electrolyte went negative
PyBaMM's SPMe predicts a negative salt concentration (-37 mol/m3) charging a low-porosity cell at 5 A; the full DFN model stays positive.
-
A zero that says why: failure reasons in the cell-design DFN re-score
The DFN re-scoring script now records whether a design scored zero because the solver crashed, stopped early or delivered nothing.
-
Does a cheaper battery model pick the wrong cell?
Searching a lithium-ion cell design directly on the full DFN model finds about 1% more energy than screening on the faster SPMe model, in the same region.